Abstract
The effect of protein concentrations on the properties of fish myofibrillar protein film (FMP) were investigated and compared with commercial wrap film (polyvinyl chloride; PVC). FMP (2 %, w/v) showed the highest mechanical properties [tensile strength: 4.38 MPa and elongation at break: 133.05 %], and water vapor permeability [2.81 × 10−10 g m−1 s−1 Pa−1]. FMP contained high molecular weight cross-links, resulting in complex film network, as indicated by lower film solubility (19–22 %) and protein solubility (0.6–1.3 %). FMP showed excellent barrier properties to UV light at the wavelength of 200–280 nm. FMP had the thickness [0.007–0.032 mm], color attributes and transparency similar to PVC film [thickness: 0.010 mm]. Therefore, protein concentration majority influenced the properties of develop FMP. The protein content of 1 % (w/v) had potential to be developed the biodegradable film with comparable properties to the commercial wrap film.
| Original language | English |
|---|---|
| Pages (from-to) | 2083-2091 |
| Number of pages | 9 |
| Journal | Journal of Food Science and Technology |
| Volume | 53 |
| Issue number | 4 |
| DOIs | |
| Publication status | Published - 1 Apr 2016 |
| Externally published | Yes |
Keywords
- Biodegradable film
- Fish myofibrillar protein
- Polyvinyl chloride
- Water vapor permeability